not required if u have approved or qualified wps/pqr in the same material as per ASME SEC IX.
 
refer sec ix article 4
 
Kevin mathew


From: BR <raghurambathula@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Monday, 18 May, 2009 7:49:06 PM
Subject: [MW:2207] Re: Socket Welding


Is it a procedure qualification or performance qualification? what is
your code of construction?

You can use groove weld qualification PQR/WQT for socket welds too,
else you may qaulify on a fillet weld test plate depending on your
requirement (2F,3F, 5F etc.)

however in general most the client/PMC doesn't allow fillet weld
qualified welders on any pressure welds. no restriction in code

On May 18, 6:03 pm, babu k <kbabu...@gmail.com> wrote:
> Hi,
>
> Is there any requirement for qualification of Socket welding?
>
> Thanks & regards,
>
> K.Babu
> Singapore

Bollywood news, movie reviews, film trailers and more! Click here.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...