Thursday, May 14, 2009

[MW:2190] Re: 2184] Ovality tolerance

It is 1% as per Section VIII Div 1 for unfired Pressure Vessels.Customer however sometimes demands stringer requirement than this.
regards
Aarpee

On Wed, May 13, 2009 at 4:12 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
if your are designing as per ASME Sec VIII div 1 pl. refer UG-80
________________________________

From: materials-welding@googlegroups.com on behalf of N Anilkumar
Sent: Wed 5/13/2009 16:03
To: materials-welding@googlegroups.com
Subject: [MW:2184] Ovality tolerance


Dear All,

Can anybody tell me,
what's the ovality tolerance of cylindrical shell pressure vessel (ID 4300 mm and plate thickness 12mm).

Regards,
Anil
























--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...