Dear All,

We are available in India for Avesta Welding & Avesta Finishing Chemical products sales & distribution.

Shriniwas Deshpande
Senior Sales Manager

Bohler Welding Group India Pvt. Ltd.
B-201 Universal Business Park,
Chandivili Farm Road,
Off Saki Vihar Road,
Saki Naka,
Mumbai 400 072. India
Ph: +91-22-2857 4448, 2857 4458
Fax: +91-22-28574445
Mob: +91 9422331958
Email: shriniwas.deshpande@bwgindia.com
Websites: www.bohlerweldinggroupindia.com
A Böhler Welding Group Company


--- On Mon, 4/13/09, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

> From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
> Subject: [MW:1930] Chemical cleaning
> To: materials-welding@googlegroups.com
> Date: Monday, April 13, 2009, 2:06 PM
> Try with Avesta their product range is very versatile
>
>
>
> Clean one (yellow) - for cleaning and degreasing
>
> Green one - for light pickling
>
> Blue one - for medium pickling
>
> Red one - for heavy pickling
>
> Finish one - for passivation
>
> ________________________________
>
> From: ---------------------------------------------
>
> Sent: Monday, April 13, 2009 2:41 PM
> To: Bathula Raghuram (Mumbai - PIPING)
> Subject: chemical cleaning
>
>
>
> Dear Raghuram
>
>
>
> Could you pl. advice me any chemical cleaning paste
> available for
> removing oxide contamination on stainless steel pipes and
> racks , it is
> better if the chemical can just clean by appying one time
> as we wanted
> to do ourself on the rig by using unskilled people to do
> this .
>
> generally we advice to go for picking and passivation for
> stainless
> steel weld joints ...
>
>
>
> Regards
>
> VM
>
>
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...