Try with Avesta their product range is very versatile

 

Clean one (yellow) – for cleaning and degreasing

Green one – for light pickling

Blue one – for medium pickling

Red one – for heavy pickling

Finish one – for passivation


From: ---------------------------------------------

 Sent: Monday, April 13, 2009 2:41 PM
To: Bathula Raghuram (Mumbai - PIPING)
Subject: chemical cleaning

 

Dear Raghuram

 

Could you pl. advice me any chemical cleaning paste available  for  removing oxide contamination on stainless steel pipes and racks , it is better if the  chemical can just clean by appying one time as we wanted to do ourself on the rig by using unskilled people to do this .

generally we advice to go for picking and passivation for stainless steel weld joints ...

 

Regards

VM


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...