you can use it for both P 1 Group 1&2 as long as notch toughness is not a requirement.

-----Original Message-----
From: materials-welding@googlegroups.com on behalf of BHARAT GOLE
Sent: Fri 10/04/2009 15:05
To: material welding
Subject: [MW:1918] Base Metal Qualifcation Range

For SMAW process as per ASME section IX PQR qualified with Base Metal A106 Gr. B to A106 Gr. B i.e P No. 1 Group1 to P No.1 Group 1

Impact & PWHT not applicable.

Please let me know what is Base Metal Qualified range for WPS...is it P 1 Group 1&2 to P 1 Group1&2 OR P 1 Group 1 to P 1 Group 1

Regards

Bharat B. Gole

_________________________________________________________________
The new Windows Live Messenger. You don't want to miss this.
http://www.microsoft.com/india/windows/windowslive/messenger.aspx

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...