[MW:1899] Re: Multi layer weld capping in SAW

Hi,
 
As per my awareness, multi layer caping in SAW to improve the toughness by way of inceasing the Volume fractin of the Accicular Ferrite in weld metal, and to avoid the over tempering of weld bead.
 
Thanks and regards,
 
K.Babu
Singapore
 

On Wed, Apr 8, 2009 at 9:27 PM, Umesan <umesan@mis.ae> wrote:

Gents,

 

Does anybody knows why multi layer weld capping, especially in sub arc welding, is preferred than single capping weld? Is there any metallurgical affect due to dilution in single layer weld capping?

 

Rgds

 


 


Maritime Industrial Services Co. Ltd. Inc. (MIS)
Corporate Office: Oilfields Supply Center, JAFZA, P.O.Box 11791, Dubai, UAE. Tel: +971-4-883-7040, Fax: +971-4-883-6484
Sharjah Operation: P.O. Box 4596, Sharjah, UAE, Tel: +971-6-528-5345 Fax: +971-6-528-5820 Website: www.miscoltd.com


The content of this e-mail together with any attachments, statements and opinions expressed herein contain information that may be private and confidential, and are intended for the named recipient/s of the mail only.

Protect the Environment ? do you really need to print this email?



Maritime Industrial Services Co. Ltd. Inc. (MIS)
Corporate Office: Oilfields Supply Center, JAFZA, P.O.Box 11791, Dubai, UAE. Tel: +971-4-883-7040, Fax: +971-4-883-6484
Sharjah Operation: P.O. Box 4596, Sharjah, UAE, Tel: +971-6-528-5345 Fax: +971-6-528-5820 Website: www.miscoltd.com


The content of this e-mail together with any attachments, statements and opinions expressed herein contain information that may be private and confidential, and are intended for the named recipient/s of the mail only.

Protect the Environment ? do you really need to print this email?







--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...