Dear ALL,
It is preferable to do UT on thickness more than 10mm.But as far material is concern there are no limitation.Only if material is course grain like casting it become difficult to do UT.Austenitic steel joints can be inspected bye UT without any problem.
regds
On Wed, Apr 8, 2009 at 2:48 PM, Rana Vikas <vhrana@gmail.com> wrote:
Dear All,Whart are limitation of Ultrasonic Examination ??Can it posible on Austenitic steel ?? if no please explain.In Austenitic steel weld joints UT posible.??In Austenitic steel plates Ut Possibel ??Great Thankful if you provide answer above questionRegardsYou friends
--
Nilesh Parsekar
Sr QC Co-ordinator
Exterran Belleli Energy
Fujairah - Sidem
Mobile - 0506561785
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
No comments:
Post a Comment