Monday, September 29, 2008

[MW:1172] Welder Qualification

yes, provided all other  variables are same per QW353
-----Original Message-----
From: SENTHILKUMAR SWAMINATHAN [mailto:skumarswami@yahoo.co.in]
Sent: Sunday, September 28, 2008 8:23 AM
To: Engineering
Subject: Welder Qualification

Hi,
I have qualified a welder as per ASME Sec.IX.
Matl: ASTM A 106 Gr B pipes,
Dia 6"X13mm in
5G position.
Process: SMAW
Same welder can qualify to weld Dia 4"X7.2mm, filling and capping only by SMAW. All other condition are same. Give the reference also in ASME IX.
 
Regards,
S.Senthilkumar



 

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...