[MW:1153] Re: SAW filler wire parameters

 
 
450-550 Amp, 30-32 V, 50cm per minute travel speed.
 


 
2008/9/19 PREM SHANKARDUTT NAUTIYAL <prem_nautiyal@rediffmail.com>

 
Dear Friends

We are presently trying to use a local make 4.8mm dia SAW filler wire (EM12K)in place of 3.15mm dia.
Can anyone tell us the correct welding parameters like:
current, voltage, travel speed,etc for 4.8mm dia wire..
The base metal is SA516Gr.70, the thickness is 70mm. The joint is single bevel groove joint with no access from other side. Presently we weld first 2 passes with TIG, Then 2 passes of SMAW and then subsequent passes with SAW-3.15mm dia. Now we want to use 5.0mm dia SAW wire. So what should be the welding parameters ? We have tried various parameters for SAW(4.8mm dia wire) but failed to get good weld finish /UT. We have a 1200A Lincoln Power source.
The joint calls for UT.

Regards

Prem Nautiyal

PREM S NAUTIYAL
CELL : 9820313278

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...