[MW:1147] welding fittings of material: St. 35.8 DIN 2448

first of all please choose appropriate subject, when posting new query, and not reply to the ongoing discussion
 
St 35.8 is normal carbon steel, you can use ER70-S2/E7018 etc.
DIN 17175 give the chem/mech composition, and DIN2448 is a dimn standard.
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]On Behalf Of Mahtab Dewan Sharif
Sent: Thursday, September 18, 2008 9:02 AM
To: materials-welding@googlegroups.com
Subject: [MW:1139] Re: Piping Materials for Hot water Tracings.

Dear All,
 
Can you suggest any suitable welding consumable for Pipes and welding fittings of material: St. 35.8 DIN 2448 with 3.1B certificate.

 

Regards
Sharif
BOC Bangladesh Limited.

 

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...