Thank You I will try to convince PMC about change to SS 304.
Kumar Bagesh
From:
Sent: Thursday, September 18, 2008 4:15 PM
To:
Subject: [MW:1141] [piping_valves] Piping Materials for Hot water Tracings.
Bhattacharyya_Bibekananda@ke0.grp.kaneka.co.jp 18/09/2008 09:08
|
|
For glycol (concentration variation, as applicable), LTCS / SS304 is
perfectly suited.
However in Pharma Plant, SS316 is also used.
Regards,
Bhatta.
kannan.sundaram@l
inde-le.com
Sent by: To
piping_valves@yah materials-welding@googlegroups.com,
oogroups.com piping_valves@yahoogroups.com
cc
09/18/2008 03:59 Subject
PM [piping_valves] Piping Materials
for Hot water Tracings.
Please respond to
piping_valves@yah
oogroups.com
The conservative material prescription for heat tracing is carbon steel. But
however you have take into account where the plant is installed, like cold
countries where the winter temp. drops quit low. This is independent of the design
temp. of the service. So refer the contract for the Min. metal design temp. for
piping, because it does vary between equipments design and piping design.
With regards,
Kannan
"Bagesh Kumar" <bagesh.kmr@gmail.com>
Sent by: materials-welding@googlegroups.com
18/09/2008 05:37
Please respond to
materials-welding@googlegroups.com
To
<materials-welding@googlegroups.com>
cc
Subject
[MW:1132] Piping Materials for Hot
water Tracings.
Dear All,
The Fluid for Industrial Heating Water is a mixture of Glycol 56 % and Water 44 %,
PMC has suggested use of Low Temperature Carbon Steel Materials,
Please Throw some light on Proper Piping Material for the said Fluid, The Design
Temperature is 130 Deg C Max and Pressure is 16 Kg/Cm2.
I have used previously SS 316, For MEG Service, Services in a petrochemical plant.
Kumar Bagesh
__._,_.___
Messages in this topic (2) Reply (via web post) | Start a new topic
Messages
Change settings via the Web (Yahoo! ID required)
Change settings via email: Switch delivery to Daily Digest | Switch format to Traditional
Visit Your Group | Yahoo! Groups Terms of Use | Unsubscribe
Recent Activity
1
New Members
Visit Your Group
Get in Shape
Find a buddy
and lose weight.
Yahoo! Groups
Share recipes
and favorite meals.
Yahoo! Groups
featured healthy living
groups on Yahoo!
.
__,_._,___ </font
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments