Wednesday, September 17, 2008

[MW:1127] Re: MS & SS welding

 
There is absolutely no problem in welding mild steel plates with
>SS304 plates. They are welded with E 309L electrodes.

Regards
Prem S Nautiyal


On Wed, 17 Sep 2008 dev yadav wrote :
>Dear All,
>
>Please suggest, is there any problem in welding of mild steel plates with
>SS304 plates.
>
>--
>DEVENDRA KUMAR YADAV
>Design Engineer
>Lars Enviro Pvt. Ltd.
>
>>

PREM S NAUTIYAL
CELL : 9820313278

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...