Is not Problems if you applicate the correct electrode (E-309) and interpass controlled 300 degree Max

carlos oliveros

On Wed 17/09/08 09:15 , "dev yadav" devendrayadav09@gmail.com sent:
Dear All,

Please suggest, is there any problem in welding of mild steel plates with SS304 plates.

--
DEVENDRA KUMAR YADAV
Design Engineer
Lars Enviro Pvt. Ltd.




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...