[MW:1104] RE: [piping_valves] Cold Bending of SS.304 1.1/2" size pipe / tube

Generally No PFHT  required for SS when cold bending is done (Hot bending is not advisable)
 
-----Original Message-----
From: piping_valves@yahoogroups.com [mailto:piping_valves@yahoogroups.com]On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Thursday, September 11, 2008 2:07 PM
To: Materials-Welding (E-mail)
Cc: piping_valves@yahoogroups.com; desaid@toyoindia.com
Subject: [piping_valves] Cold Bending of SS.304 1.1/2" size pipe / tube

You may use Table UHA44 (ASME Sec VIII div1) for PFHT requirement, which is most common in HE  U tubing.
Para 331.4.2 not clearly spelt out for P8 material, but there is something called 10% strain limit, which is same as given in UHA44 for 304 material
 
 
From Dhwani Desai........

desaid@toyoindia.com

11/09/2008 03:53

To
Kannan.Sundaram@Linde-LE.com
cc
Subject
Cold Bending of SS.304 1.1/2" size pipe / tube


Hi,

Is there any code restriction for doing cold bending of SS-304 (1.1/2") pipe? Any post bending heat treatment required?
31.3 only specifies heat treatment for ferritic steel.


thanks & Regards,

Dhwani
 

__._,_.___
.

__,_._,___

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...