ST52.0 which is equivalent to 1.0421 / A519 and ST52-3N which is equivalent to 1.0570/1.0576 / A516, A572 can be used for the purpose inline with B31.8 para 811.221 being an official equivalent of ASTM material.

With regards,
Kannan



"Mohammad Yaghoubi" <yaghoubi_m@nigc.ir>
Sent by: materials-welding@googlegroups.com

11/09/2008 12:07

Please respond to
materials-welding@googlegroups.com

To
materials-welding@googlegroups.com
cc
Subject
[MW:1097] MATERIAL APPLICATION






DEAR SIR
CAN WE USE PLATES OF DIN1629 ST 52.0 OR DIN17121 ST52.3N TO MANUFACTURE
SPLIT TEE ACCORDING TO ASME B31.8
BEST REGARDS
MOHAMMAD YAGHOUBI


----------------------------------------------
National Iranian Gas Company
http://www.nigc.ir




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...