[MW:1084] Re: Current consumed in 1 inch dia welding

Dear,,
your question is not clear,,,current varies with the diameter of electrode..So what material you want to weld & what diameter of electrode you want to use..

On Sat, Sep 6, 2008 at 4:03 PM, Mahuri Snehkumar (TIPO - QA/QC) <S.Mahuri@panipat.ticb.com> wrote:

Dear all,

Can any one tell me for 1 inch dia welding what would be the current consumption?  Any thumb rule or some sort of formula.

 

Regards,

 

Snehkumar L Mahuri

Lead NDE & Welding

M : 9215989508

 






--
Regards,
Harish katesia
Mob no.09725016042


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...