Thursday, January 5, 2017

[MW:25872] Re: Dissiminal welding between aluminum alloy and stainless steel

You may use friction stir welding

On Monday, December 19, 2016 at 5:53:43 AM UTC+3, duynhat240685 nguyen wrote:
I am researching on the dissimilar welding materials by using TIG and MIG welding method. But I don't know, how to calculate the welding parameters? please help me. 
Thank you so much!

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/884dd743-2cfd-4d5c-a902-4f5e25fc3770%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.