Ali,
 
You can reveiw the MTC with latest SecII and certify if all the content of MTC meets the code  requirements. Mentionging MTC has been revewied with ASME SEC II Edition---- and found acceptable and same cane be recertified by the AI.
On Tue, Apr 16, 2013 at 8:04 AM, Mhaskar Aly <mhaskar.aly@gmail.com> wrote:

Dear Experts

We wanted to use SA516 Gr70 plate from DANSTEEL (MTCs' are attached) where original marking on plate is as follows

UR

LR EH36 S355K2+N CE; refer the attachment

(SA516 65/70MTLTV is not punched on plate; but the marking on plate is traceable to given mtc…

Mtc shows Specification as ASME SA516 65/70 LR EH36 S355K2+N

Mill has issued letter regarding modification of marking as ASME SA561 65/70 MT LTV…(refer attachment)

We internally released these plates as marking on plate is traceable to MTC…further there is letter from Mill regarding the marking.

Kindly advise can we use this plate for ASME U Stamped Pressure vessel job 

 

Ali

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...