Re: [MW:17421] Ultrasonic testing of fillet weld joint.

Dear Friend,
In general there is no limitation for ultrasonically testing of fillet welds by normal and angle transducers (if you can position the probe on desired surfaces and those are accessible), but the issue is which kind of defect you are looking for and where you are expect them?
For example, if you are looking for incomplete fusion in the side wall of the joint, so there is no problem but if you are looking for root pass defect, it is more complicated (I will not say impossible) and need more experience.

Regards



On Mon, Apr 15, 2013 at 9:45 PM, manoj john <manojacgnr@gmail.com> wrote:
Dear members,

Is it possible to carry out ultrasonic test on the fillet weld of nozzle RF pad to shell and fillet weld joint (without bevel) of built up beam.  

Thanks in advance.
Manoj.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...