Tuesday, April 16, 2013

Re: [MW:17421] Ultrasonic testing of fillet weld joint.

dear sir
if the joints are full penetration fillet welds , then we can do the UT  for the welds. otherwise  if  you scann the weld defect eco will be observed for partial penetration welds.
regards
GSR


On Mon, Apr 15, 2013 at 10:45 PM, manoj john <manojacgnr@gmail.com> wrote:
Dear members,

Is it possible to carry out ultrasonic test on the fillet weld of nozzle RF pad to shell and fillet weld joint (without bevel) of built up beam.  

Thanks in advance.
Manoj.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:26652] ASME Tack welder Qualification

You are wrong. When Asme is applicable and wenn tack welds are to be removed no need for qualification  Sent from my Samsung Galaxy smartpho...