Wednesday, April 3, 2013

Re: [MW:17279] Welding of E316L material -Reg

Yes you can use 316-16 for 316L material
You can also use 316-15 if it involves very low temperature charpy,
316-17 is better but it is not highly suitable for 3g welds as the weld metal is very fluid and welder skill is very important.
316-16 is good as it serves all purpose and all position.
 
Hope the info helps
 
From: siva subramanian <ian_siv@yahoo.co.in>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, 1 April 2013, 23:01
Subject: [MW:17261] Welding of E316L material -Reg

Dear sirs,
                 I have one clarification regarding welding of SA240 GR 316L material.
May I use E316-16 to weld 316L material.If it is not possible means What is reason behind?

Please Clarify me.

Always Thankful,
A.Sivasubramanian
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...