Was this checked earlier with the different method, using OES type equipment
of another XRF instrument?
On Wed, 12 Sep 2012 08:38:57 -0700 (PDT)
Raghuram Bathula <raghurambathula@gmail.com> wrote:
> Which is machine you have used initially?
>
> On Sep 11, 2:30 pm, mohamed jubair
><kmd.jub...@gmail.com> wrote:
>> Dear All,
>>
>> Thanks for all your valuable suggestions.We checked with
>> other(INNOV-X-Systems) PMI equipment and got positive
>>results.We have done
>> 100% checking and all joints found as T91.Once again I
>>thank you all for
>> your suggestions.
>>
>> Regards
>> Jubair
>
> --
> To post to this group, send email to
>materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
>materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at
>http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members
>personel views and meant for educational purposes only,
>Users must take their own decisions w.r.t. applicable
>code/standard/contract documents.
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment