Dear Rinshad,
--
-- We have faced this problem before within quarry installation, its whether due to:
1- Wire diameter Vs used type of gravel. Please give the max material size that could go against this screen
2- Rubber special roll, shall be placed underneath the screen generally U grooved type. Hence no shear is stand by the screen's wires.
But if you have faced this problem just after crimping and before any screening use this is purely material Vs crimping inappropriate process.
See Haver&Boecker Process for Crimping, it might be of use.
Lassaad
2012/9/1 rinshad abdul rahman <rinshad043@gmail.com>
Dear All,--The photo attached herein showing the wire for screening meshes,we are facing the problem of cracking of wire after the crimping (a process which is to make meshes from wire).Can anybody suggest any test method to determine the reason of cracking ?Is it have any ASTM methods are available ?The standard for producing the meshes are the followingBS 7372:Part 3 /ISO 4783-3 - Choice of aperture size and wire diameter combinations for industrial wire screens and woven wire cloth.DIN 1SO 14315 - Industrial wire screens technical requirement and testing.The chemical and mechanical properties are conform to DIN 17223 Part 1 class A.Thanking you in advance
Rinshad
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Meilleures salutations
http://www.linkedin.com/pub/lassaad-mokrani/16/364/907
P Pensez environnement! N'imprimez ce mail que si c'est vraiment nécessaire
Please consider your environmental responsibility before printing this e-mail
This e-mail is confidential and it is intended only for the addressees. Any
review, dissemination, distribution, or copying of this message by persons
or entities other than the intended recipient is prohibited. If you have
received this e-mail in error, kindly notify us immediately by telephone or
e-mail and delete the message from your system. The sender does not accept
liability for any errors or omissions in the contents of this message which
may arise as a result of the e-mail transmission
MOKRANI Lassaad
Consultant Civil Engineer
Tunisia
00216 20 649 755http://www.linkedin.com/pub/lassaad-mokrani/16/364/907
P Pensez environnement! N'imprimez ce mail que si c'est vraiment nécessaire
Please consider your environmental responsibility before printing this e-mail
This e-mail is confidential and it is intended only for the addressees. Any
review, dissemination, distribution, or copying of this message by persons
or entities other than the intended recipient is prohibited. If you have
received this e-mail in error, kindly notify us immediately by telephone or
e-mail and delete the message from your system. The sender does not accept
liability for any errors or omissions in the contents of this message which
may arise as a result of the e-mail transmission
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment