Dear all,
As a senior expert in MMA-electrodes since many years at Esab, I can confirm that E6013-electrodes shall not be rebaked or heated in any way. When manufactured, these electrodes are dried at a temperature below 100 °C. This is necessary in order to achieve a good binding of the coating. The final moisture content in the coating is around 1%, which is necessary for the welding properties. The coating also contains a sizable amount of organic material and water containing minerals. The coating moisture will vary with the moisture of the ambient atmosphere, normally within permissible limits.
It is recommended to store these types of electrodes under the same conditions as other types of electrodes, i.e. dry and protected conditions, in order to avoid any unnecessary rusting of the wire or coating damage.
Best regards,
Claes Gillenius
Development Engineer, MMA. (Spec. stainless and non Fe-alloys)
Direct tel: +46 (0)31 509315
Mobile +46 (0)707532012
Company ESAB AB
Address Box 8004, 402 77 Gothenburg, Sweden
Lindholmsallén 9
Company reg number 556005-7738
mahendran p <pmahe_79@yahoo.co.in> Sent by: materials-welding@googlegroups.com 2010-06-08 08:03
|
|
Dear Mr.Phil, Does it require any holding temperature? I ever read in one std/code but not sure. Thanks. P.Mahendran. --- On Mon, 7/6/10, Phil.Chew@esab.net <Phil.Chew@esab.net> wrote: From: Phil.Chew@esab.net <Phil.Chew@esab.net> Subject: Re: Re: [MW:5421] storage condition of E6013 To: "materials-welding" <materials-welding@googlegroups.com> Date: Monday, 7 June, 2010, 12:30 PM I am an ESAB employee and I can confirm that you should not bake a E6013 stick electrode This is a rutile type electrode and does not require baking Best Regards PHIL CHEW Global Segment Manager -Transport ,Shipbuilding,M&R ESAB Holdings Ltd, 322 High Holborn, London, UK, WC1V 7PB Tel: +44 (0) 7584 219132 email: PHIL.CHEW@esab.net ESAB Holdings Ltd is a company registered in England and Wales . Co registration no 1687590 Registered Office: 322 High Holborn, London , UK , WC1V 7PB www.esab.comPlease consider the environment before printing this email. From: sugu puma [pumamy@yahoo.com] Sent: 06/06/2010 07:21 MST To: materials-welding@googlegroups.com Subject: Re: Re: [MW:5416] storage condition of E6013 are they sure you said cannot baking in oven..............?,what the manufacture recommendation said? From: john rodrigues <johnrodrigues2@rediffmail.com> To: materials-welding@googlegroups.com Sent: Sun, June 6, 2010 3:39:15 PM Subject: Re: Re: [MW:5412] storage condition of E6013 Hello, E6013 is rutile type electrode and it does not require baking. Regards. joh On Sun, 06 Jun 2010 09:09:34 +0530 wrote >Dear all, The baking temperature is 350 - holding temperature 150,see the manufacture rules and regulations before open the box of electrode cartoon,this is all low hydrogen electrode using,followup according manufacture recommendation and also take look in AWS D1.1. From, M.Sugumar From: Sandeep Kp To: materials-welding@googlegroups.com Sent: Sat, June 5, 2010 10:34:30 PM Subject: [MW:5401] storage condition of E6013 Dear all, Let me know the baking & holding temperature of E6013 electrodes of ESAB. Regds, Sandeep.k.p -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -- > To post to this group, send email to materials-welding@googlegroups.com > To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com > For more options, visit this group's bolg at http://materials-welding.blogspot.com/ > The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. > John Rodrigues -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. ______________________________________________________________________ This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it. ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof. -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. |
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
______________________________________________________________________
This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it.
ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment