Hello
 
To me there is not difference, is just a matter of semantics, the two seek to know if it leaks and resist the pressure pipe.
ASME B31.3 I know, too seeks to verify the strength of the pipe. if is not good also would have leaks. Finally is same scope

Agustin



De: hpi001 <pieper-qsi@kpnmail.nl>
Para: Materials & Welding <materials-welding@googlegroups.com>
Enviado: vie, junio 18, 2010 4:44:42 AM
Asunto: [MW:5646] Re: Hydrostatic pressure testing of piping systems - is it for leak test or for strength test ?

Dear Rahul,

The proof test as mentioned by PED and EN is for proving the
constructions strength and depending on the design rules test pressure
will be about 1.3 - 1.4 times the maximum design pressure and mostly
will run for about 1/2 till 1 hour.

On the other hand the leak test is for proving the structure /
pipeline has no leaks. This does not only consists the piping /
pipeline itself but also al flange connections present in a system and
the applied gasket material.
This leak test is often not mentioned in design codes but mostly a
customer requirement, I have to mention that I'm not known with the
content of ASME B31.3.
Test pressure as well as test duration depends completely on clients
requirements . I know that for pipelines often 24 hours is taken as
test duration. The maximum pressure drop allowed should be agreed in
front of the test but is mostly also specified in client requirements.

Hope this clarify things for you.

Best Regards,

Herman Pieper

On 18 jun, 10:53, "Pisat, R. (Rahul)" <Rahul.Pi...@akzonobel.com>
wrote:
> Hello All,
>
> I have one question regarding scope of Hydrostatic pressure testing of
> piping systems.
>
> As per ASME B31.3, Hydrostatic pressure testing of the piping systems is
> defined as Hydrostatic leak test ie to check each piping system to
> ensure tightness.
>
> The PED (97/23/EC) guidelines & EN 13480 pressure piping code ask for
> PROOF TESTING, ie by Hydrostatic testing, of the piping systems to check
> the Strength & Integrity of the piping systems.
>
> Why there is such difference between the approach/aspect of Hydrostatic
> testing ?
>
> If in 31.3, Hydrostatic pressure testing is only defined for check the
> tightness ? how can one satisfy the PROOF TEST requirement of PED for
> ASME B31.3
>
> Your kind replies will be highly appreciated.
>
> Kind regards
>
> Rahul

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...