We require an electrode that is compatible with the higher strength and toughness of A517 Grade F, and 
It should also maintain a good weldability with A537 Class 2. 
E11018 is preferable for welding A517 Gr F, A537 Cl II, or dissimilar joints, as it matches the strength 
and toughness requirements of both materials and is designed for high-strength, low-alloy steels.  
E9018M is suitable for A537 Cl 2, and provides good toughness but may not meet the impact requirements 
for A517 Gr F at low temperatures.   
Use an appropriate preheat (150°C–200°C) as per welding codes to avoid hydrogen-induced cracking 
and interpass temperature (200°C) to control overheating.

C Sridhar.

On Sat, 19 Jul 2025 at 18:35, Ali Sherif <ali.sherif10@gmail.com> wrote:
E9018M will be suitable

On Sat, Jul 19, 2025 at 3:40 PM Maharajan Subramanian
<ma10ja23@gmail.com> wrote:
>
> Dear experts,
>
> In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.
> For A517Gr.F using E 11018M and A537CL-II using E 9018M.
> Only one joint have a A517Gr.F with A537CL-II.
> Which Electrode is better for PQT.
> Your valuable guidance is highly appreciated.
>
> Thanks with regards,
>
> S.Maharajan.
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALiLA%3DcV4G6_ZJi7Y16RfnHxC8mz%3D3Z%2B4a7DGXFaE2vafWWuTw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFc%2BNSQztk_A7F45wo64%2BiPwR%3DrcxQULSmVTiS7%3D6J91c5%2B%3DjQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYihzZFv6W%3DD8Der6fk5hEAV3zbdHY8ig9%2BxpLJKwJ0uoOw%40mail.gmail.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...