Skip to main content

Re: [MW:35708] ThicknessRange of wps

If it's P8, won't a PQR qualified on 6mm thick cover the welding of this dis-similar thickness (QW-202.4)considering welding deposit thickness of 10mm?
 Regards,
Michael 

On Sat, Jun 28, 2025 at 12:02 PM Pravin Kurade <pravinkurade@gmail.com> wrote:
In this case it's dissimilar thickness and considering its P8 you need 20 mm thk welding procedure which will cover both the range I assume impact test not required. 
Thanks with Regards....

Pravinkumar Kurade

ASME Authorized Inspector (National Board-15396), 
Repair Inspector (NBIC) R-Endorsement,
PED Inspector, DOSH Inspector,
B.E. (Mech.), Lean Six Sigma Green Belt,
C-SWIP-3.1 (Welding Inspector - UK)
ASNT Level II - MT, PT, RT , VT, LT
Mob : +91 8484848029

On Sat, 28 Jun, 2025, 9:25 am israr ahmed, <ahmedisrar.nm@gmail.com> wrote:


dear team
What should be the range of qualification if we are welding sight glass thickness 40mm with shell of 10mm?

Israr Ahmed Noor Mohammed
+919930308261

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEJoza%2Bw8YOMSuBzMnVCePwFuvbJDVm6AtKDh0AhGZtmpqTHmw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAM02rkfO--fp%2B7vbFR737qW17dVoTkmvQQbPd36THjHn5Ti2-w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFxNsAGdA1RJd0hQ%3D%3DnxoWTx_6bbuSDjw%2Bg%2B2O98SgzhPWNkXQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .