ASTM A297 Grade HP (Cr 24-28% & Ni 33-37%) is a heat-resistant stainless steel casting alloy commonly used in high-temperature 

applications. ASTM A297 Grade HP (ASME sec II Part A and its UNS number is N08705) does not have a direct, one-to-one equivalent 

in ASME standards and modified slightly for specific applications (example: pressure vessels, piping).


For practical purposes, in ASME codes, Grade HP would be referenced under SA-297 Grade HP for applications like furnace parts, heat 

treatment equipment, or other high-temperature cast components. For a specific purpose like piping, it is referred to as ASME B16.5 -for 

flanges.


C Sridhar.

-------------------------------------------------------------------------------------------------------------------------------------------------


On Thu, 24 Jul 2025 at 14:45, 'K Dinesh' via Materials & Welding <materials-welding@googlegroups.com> wrote:
ASTM A297 Gr. HP

Thanks & Regards

K.Dinesh 

Metallurgist


P.O. Box 1197, P.C 130, Muscat, Sultanate of Oman

Tel:  +968 24501524, 24505590 (Ext.42), Mob: +968 99880633, Fax: +968 24503814

Email: dinesh@lonestaralpha.com , Web: www.lonestaralpha.com , Location: Click here for Location Map

Locations: Muscat, Sohar, Duqm, Salalah & Liwa

Lonestar now does Pesticide Residues Testing in our new facility at Liwa!

 Consider your environmental responsibility. Think before you print.



On Wed, Jul 23, 2025 at 7:51 PM Vishwas Keskar <vvkeskar123@gmail.com> wrote:
What is ASME material grade?



On Wed, 23 Jul 2025 at 11:08 AM, 'Dinesh K' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi,

We are going to do PQR testing of heat-resistant steel tubes. Client has given a reference of QW-466.19 for the bend test, which i could not find in the latest ASME IX. 

Can anyone please help

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/732729f5-daa4-47f0-be88-367ad78c960bn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADder3PKdVJ45xOrwVAkekeMCPTNMjBvpF_EiRg1A8m%2BEV9PcA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG5OBYGGbwwjMuWpKjF8nf21F%3DWQ2SUDh%3D6DBY9_-n9m2sE3Fw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYiiypAFmkBtU0Yt5W_ReGTjY1unnmZiXshk8ffehKm0TvA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...