Re: [MW:35714] PPM to mg/m2 conversion

 3000ppm =   50μg/cm²
(As per Elcometer kit 130 datasheet. Ref:- https://www.elcometer.com/en/elcometer-130-salt-contamination-meter.html)

1 μg/cm² = 10mg/m² 

On Tuesday, March 29, 2022 at 10:47:33 AM UTC+3 Muhammed Ibrahim PK wrote:
1ppm how much mg/m2?.
Is there any conversion formulae?

Reg,
Ibrahim

On Mon, 28 Mar 2022, 9:36 am 'james gerald' via Materials & Welding, <material...@googlegroups.com> wrote:
Please correct it as 2000ppm

Thanks & Regards

J.Gerald Jayakumar




On Monday, 28 March, 2022, 09:55:17 am GMT+4, james gerald <gerr...@yahoo.com> wrote:


1% is 10000 ppm and it must be 20ppm, please check

Thanks & Regards

J.Gerald Jayakumar



On Monday, 28 March, 2022, 07:14:50 am GMT+4, Muhammed Ibrahim PK <ibra...@gmail.com> wrote:


Gents,

Is there any conversion available for ppm to mg/m2?

For Aramco projects, the chloride content measured in ppm using bresle patch kit in ppm.

As per Aramco spec the acceptable range is 20mg/m2.

Couldn't find the conversion. If anybody can advice, it will ne highly appreciated

Reg,
Ibrahim

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmNqFyBdfAsrXAfykfbe4-Yw%2B0hZHYxmrDWA8uHC5WUiow%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/a6ebf8ed-2611-434e-b07b-2888e02dd860n%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...