Skip to main content

Re: [MW:34476] Requirement of separate PQR for Low Alloy steel materials

Vishwas,

Do we need simulation production coupon for Repair.

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 9 August, 2023 at 09:45:01 am IST, Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:


Then no new PQR can be used 
Follow /comply all supplementary essential variables 
Vishwas -IWE
On Thursday, August 3, 2023 at 8:49:41 AM UTC+5:30 ranajit chatterjee wrote:
PQR holing time - 2 hrs.
Same holding time for production job.

Regards,
Ranajit Chatterjee


From: Vishwas Keskar <vvkes...@gmail.com>
Sent: Wed, 02 Aug 2023 08:37:56
To: material...@googlegroups.com
Cc: chatterje...@yahoo.com
Subject: Re: [MW:34454] Requirement of separate PQR for Low Alloy steel materials

What is holding time of your existing PQR ?
What is holding time of your production job?
 
Vishwas IWE
 
Sent from my iPhone
 
On 01-Aug-2023, at 7:02 PM, 'ranajit chatterjee' via Materials & Welding <material...@googlegroups.com> wrote:
 
Dear Friends,

Please express your advice for any separate PQR required for Low alloy(P4/P5A/P5B) materials after weld repair (1/2 times) any weld defects where PWHT cycle applicable?
Waiting for your expertise reply.

Regards,
Ranajit Chatterjee

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20230801115929.5690.qmail%40f5mail-224-129.rediffmail.com.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/e7b43fc0-aecc-4c0b-ba50-2a3f1f5bf184n%40googlegroups.com
.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...