[MW:34480] Details of wleding grove and gap

Dear Sir's
Can Anybody clear that for 10mm thickness plates how much root gap with back strip to be made as per ISO9692-1 and in this stanrd showing >16mm but it is 10mm plate so that i m doubt about this. 
so that can anybody help in this regard



H .PAMPANAGOUDA.PATIL| (CRS&I-SHOP) | Vijayanagar Works | JSW Steel Limited
P.O. Vidyanagar  | Dist. Bellary  | Karnataka-583275 | India
Direct : +91 8395 243105
Cellphone: +91 9480694735
Email : pampanagouda.haraginadoni@jsw.in 
Website: www.jsw.in
P Print only when necessary |7 Switch off as you go |qRecycle always
#Better Everyday


Confidentiality Notice

The information  contained in this electronic message and any attachments to this message are intended  for the exclusive  use of the addressee(s)  and may contain  confidential  or privileged information. If you are not the intended recipient, please notify the sender at JSW  or  System Manager ( admin@jsw.in ) immediately  and destroy all copies of this message and any attachments.  Recipients must check this email and its attachments  for the presence of viruses before downloading them. JSW Group accepts no liability for any damage caused by any virus transmitted by this email.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACMHz4WBHnfx8Pndh31gaaFB0oVoDwFpC7LcVLweOpXkbbwHgA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...