Re: [MW:34372] S195T (1.0026) material equivalent material in astm ?

Dear Madheswaran,

S195T is C-Mn Steel with Material No. 1.1 as per EN 15608,

You can consider it as P1 G1 

On Tue, Jun 27, 2023, 08:41 Madheswaran s <madhes.sss@gmail.com> wrote:
Dear All, 

I have WPS P1 material , S195T (Carbon steel) is tubing/Piping material client free issue material. I don't know the P number for this material, I seached in google , i didn't get any equivalent material in astm/Asme for determinig P Number. Can anyone clear the issues briefly?

Can i use same WPS for that of P1 material or I have to qualify for S195T as a new.? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1be202d9-fb44-41d9-9fd8-5afa8d36708bn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zfTMMWHvQKvVR%2BNOSF_e2fUsiBZWtWpXxTHEitt_CxbhA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...