Skip to main content

Re: [MW:34361] Crack Repair

1. Pre-Weld Inspection: Inspect the cracked area to determine the extent of the damage and verify that it can be repaired through welding. If the crack is extensive and compromises the structural integrity of the material, you may need to perform a metallurgical replica to determine if it's feasible to repair or if the material needs to be replaced.

2. Crack Removal: Remove the cracked area by grinding or gouging the crack using an angle grinder or a carbon-arc gouging technique. Ensure complete crack removal and create a smooth, gradual transition along the edges of the groove.

3. Surface Preparation: Clean and prepare the area to be welded by removing rust, paint, oil, grease, or any foreign contaminants. Ensure that the groove sides and surrounding areas are free from defects or damage like gouges, sharp edges, or overcuts.

check with PT/MT for remaining nonvisible defects 

4. Preheat: Preheat the base material following the base material manufacturer's guidelines or the welding procedure specification (WPS). For SA 516-Gr 70, the preheat temperature is typically between 150°F to 300°F (65°C to 150°C) depending on the thickness of the material and the welding process being used. The preheat should be maintained throughout the entire welding process.

5. Welding Procedure Specification (WPS): Follow an approved Welding Procedure Specification (WPS), which defines the welding parameters, filler metal, and welding techniques to be used for the repair. For SA 516-Gr 70, a suitable filler metal can be a low hydrogen electrode, such as AWS E7018 or E7016.

6. Welding Technique: A suitable welding technique should be chosen based on the WPS, e.g., Shielded Metal Arc Welding (SMAW), Gas Metal Arc Welding (GMAW), etc. Properly position the workpiece and apply the welding technique following the appropriate sequence and deposition rates. 

7. Interpass Cleaning and Inspection: Between each weld pass, clean the weld bead by wire brushing or grinding to remove any slag or impurities. Inspect for any defects or discontinuities.

8. Post-Weld Inspection: Upon completion of the welding, visually inspect the weld for any noticeable defects or irregularities. Further inspections might be necessary, such as dye penetrant testing to confirm the absence of Ʃventuel appearance of other crack.

If you are really interested on repair methods check NBIC Inspection Code Part 3 and ASME PCC-2

Δρ. Ī“ĪµĻŽĻĪ³Ī¹ĪæĻ‚ Διλιντάς
Ηπείρου 5 , Μελίσσια - 15127
Αεροναυπηγος ĪœĪ·Ļ‡Ī±Ī½Ī¹ĪŗĻŒĻ‚ - ĪœĪµĪ»ĪæĻ‚ ΤΕΕ 55018
Τηλ +30 210 8100578, +30 6944 646 204

Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I,  Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis


Στις Τετ 21 Ιουν 2023 ĻƒĻ„Ī¹Ļ‚ 1:57 μ.μ., Īæ/Ī· Mostafa DAIF <mostafa.daif@taqamorocco.ma> έγραψε:
To implement a repair to a crack on a base material SA 516-Gr 70, you must follow a proper welding procedure which includes the following steps:

1. Pre-Weld Inspection: Inspect the cracked area to determine the extent of the damage and verify that it can be repaired through welding. If the crack is extensive and compromises the structural integrity of the material, you may need to perform a metallurgical replica to determine if it's feasible to repair or if the material needs to be replaced.

2. Crack Removal: Remove the cracked area by grinding or gouging the crack using an angle grinder or a carbon-arc gouging technique. Ensure complete crack removal and create a smooth, gradual transition along the edges of the groove.

3. Surface Preparation: Clean and prepare the area to be welded by removing rust, paint, oil, grease, or any foreign contaminants. Ensure that the groove sides and surrounding areas are free from defects or damage like gouges, sharp edges, or overcuts.

4. Preheat: Preheat the base material following the base material manufacturer's guidelines or the welding procedure specification (WPS). For SA 516-Gr 70, the preheat temperature is typically between 150°F to 300°F (65°C to 150°C) depending on the thickness of the material and the welding process being used. The preheat should be maintained throughout the entire welding process.

5. Welding Procedure Specification (WPS): Follow an approved Welding Procedure Specification (WPS), which defines the welding parameters, filler metal, and welding techniques to be used for the repair. For SA 516-Gr 70, a suitable filler metal can be a low hydrogen electrode, such as AWS E7018 or E7016.

6. Welding Technique: A suitable welding technique should be chosen based on the WPS, e.g., Shielded Metal Arc Welding (SMAW), Gas Metal Arc Welding (GMAW), etc. Properly position the workpiece and apply the welding technique following the appropriate sequence and deposition rates. 

7. Interpass Cleaning and Inspection: Between each weld pass, clean the weld bead by wire brushing or grinding to remove any slag or impurities. Inspect for any defects or discontinuities.

8. Post-Weld Inspection: Upon completion of the welding, visually inspect the weld for any noticeable defects or irregularities. Further inspections might be necessary, such as dye penetrant testing to confirm the absence of Ʃventuel appearance of other crack.

Best regards,

Le mar. 20 jui. 2023 Ć  13:09, Ashish Chacko <iamashleo007@gmail.com> a Ć©crit :
Unfortunately i cant share the sketch. Base material is SA 516-GR 70 and clad material is SS 347.And the service is NG saturator.
On Tuesday, 20 June 2023 at 11:56:31 UTC+3 Ahmed Eissa wrote:
Dear Sir, 

Please provide sketch of Crack location and Materials grade and service of the HE. 
Thickness and if any of API 934 series apply 

Thanks 
On Tue, Jun 20, 2023 at 10:48 AM, Ashish Chacko

Request for Expert Advice on Crack Repair

I am writing to request the support of the experts out here on a crack repair in an exchanger. The exchanger has a fillet weld with the shell, and a crack was found during the last TAM. There is a possibility that the crack will be found again during this TAM.

The base material of the exchanger is 58mm P1 (A516-GR 70) with cladding of SS347 of 6mm. There are two scenarios to consider:

  • Scenario 1: Localize repair of the ring chamber fillet weld by grinding and welding. The client is requesting for annealing after the repair. Is this really required?
  • Scenario 2: If the crack propagates to the shell, the client is asking for DHT and PWHT. When should DHT be performed, before or after the cladding weld? Is there any exemption for PWHT?

I would be grateful for any advice that you can provide on these two scenarios. Thank you for your time and consideration.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4010c4b0-e975-43fb-8399-b75840f3fc24n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c8b0c412-fb78-400e-91d2-7f29e17c934cn%40googlegroups.com.
--

Mostafa DAIF
Chef preparateur

T : 05 23 38 90 72
M : 06 61 54 12 95
TAQA MOROCCO PB 99 Sidi Bouzid - El Jadida 24 000 - Maroc
taqamorocco.ma

TAQA MOROCCO is a member of the Abu Dhabi National Energy Company Group of companies.
  

The information contained in this communication is confidential, may be attorney-client privileged, and is intended only for the use of the addressee. It is the property of Abu Dhabi National Energy Company PJSC (TAQA) or one of its affiliates. Unauthorized use, disclosure or copying of this communication or any part thereof is strictly prohibited and may be unlawful. If you have received this communication in error, please notify me immediately by return email and destroy this communication and all copies thereof, including attachments.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANRRH0JVz51_3StjR8FjHC_AGenZ8sqsfdsYiEFSJ8S22J1%2BEQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40D7msnJMViJ3k97W7k7YPCwAuQ30rUU2S%3DJVd%3D6euuenQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...