Friday, June 16, 2023

Re: [MW:34334] Changing filler from er316l to er308

u can, but generally when u prepare WPS, u can mention like 308 for 304, 316 for 316 etc in single wps except where Ano changes
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Jun 15, 2023 at 3:21 PM Shaik Meraj <123shaikmeraj@gmail.com> wrote:
Dear Experts

We have prepared SS PQR with 316 PIPE and ER316L filler

Right now we have project of SS304 to SS304 1 1/2"pipe welding for flocculant service.

As changing filler classification from PQR to WPS is supplementary variable as per ASME SEC IX.
 
Can I use my SS PQR 316 to prepare wps for ss304 to ss304 by changing only filler material to er308 (in pqr it is er316L) as both material falls in same P no and group no.

Can I strongly justify my point of changing filler classification er316L to er 308 in wps without undergoing any additional testing or procedures.

Kindly suggest the strong points with standards if any.

Thank you in advance 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/179b6dd3-2ea8-4fe8-b718-8890c6d9d1e4n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNrTB7q_6uev8Z0yLr%2BA4q_P_8AWq2NN3c51NoYS_xVpw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...