Please check design temperature and fluid service, if impact test requirement you can not do. if impac test requirement you can do that. 

Vào Th 5, 15 thg 6, 2023 vào lúc 12:51 Shaik Meraj <123shaikmeraj@gmail.com> đã viết:
Dear Experts

We have prepared SS PQR with 316 PIPE and ER316L filler

Right now we have project of SS304 to SS304 1 1/2"pipe welding for flocculant service.

As changing filler classification from PQR to WPS is supplementary variable as per ASME SEC IX.
 
Can I use my SS PQR 316 to prepare wps for ss304 to ss304 by changing only filler material to er308 (in pqr it is er316L) as both material falls in same P no and group no.

Can I strongly justify my point of changing filler classification er316L to er 308 in wps without undergoing any additional testing or procedures.

Kindly suggest the strong points with standards if any.

Thank you in advance 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/179b6dd3-2ea8-4fe8-b718-8890c6d9d1e4n%40googlegroups.com.


--
Best & Regard
Pham Thanh Tinh
QC Manager
China National Chemical Engineering Third Co.LTD
South Ghawar Gas Separation Plant & Associated Facilities Project
Mobile phone +966. 556802308 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEVAJwaxZNDfO%2B4s4UN4FZkbHmh%3DaJviFfDywervX5tcUQstNg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...