Thursday, June 15, 2023

Re: [MW:34329] Hydro failure

Dear Sudipto
what is the location of failure, weld, HAZ, BM (which side)? NDE may not detect minute linear flaws, you need run full failure investigation on samples at laboratory, 

On Thu, 15 Jun 2023 at 15:21, 'sudipto banerjee' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi All,
One LTCS ASME DIV 1 vessel failed in Hydrotest in the joint of 2"LWNRF with Body blind flange. Its a set on type welding.
Nozzle is of SA 350 Gr. LF2 CL1 (16.7 thk) and the body blind flange of SA 765 Gr II (117 thk).
The UT test of the joint shows satisfactory.

Can anyone tell what cud be the possible reasons pls.

Thanking You.
I remain.

Best Regards,
Sudipto Banerjee, BE (Mech.), C.Eng. (India), FIE

Mobile UAE: +971(0)503946212
Mobile India: +91 9987561673 (Whats app no.)

--

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubkwCdpydT_-e-%3DCNp%3DVefAnbdn%2BrpSYjZxvFZHkXhdOJg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...