Re: [MW:34322] using API 1104 qualified PQR with ASME sec IX WPS

What is ur construction code pleas let me know.

On Wed, 14 Jun 2023, 13:07 aravind roche, <aravindroche@gmail.com> wrote:
Dear Experts,

please provide the reference we have API 1104 qualified PQR, can we write new WPS with ASME sec IX.

If you have reference please provide me.

Aravind.A

  

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ffbf934a-b2f8-4db8-9118-1fb6045d71c9n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEML-XQ7V2-7Sx610EDXEvfdEv5eCZCWN9nPBfjA_QpSfw98qg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...