dear sir,

Please tell me where it is mentioned "based on product like plates, 0.2%, For tubular products--2%".


On Mon, Jun 12, 2023 at 11:49 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
based on product like plates, 0.2%, For tubular products--2%
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Jun 12, 2023 at 8:37 AM Ganesh R nair <ganeshrnair9@gmail.com> wrote:
Dears,

As per SAEP - 324, linear weld rejection rate for welder is 0.2% max. But as per SAES W-10, maximum weld repair rate for welder is 2%. Which is correct. I am attaching screen shot of SAEP-324 and SAES W-10. Please advice.

Thanks & Regards,
Ganesh R

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ_8oJVEM1gb7b6ahL6ma0%3DndfA247w5OwNyOVKE73aidhdz3A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO%3DrUkKjAzmDUZCRy5XRYfEW%3Deax%3DC13a8356PKf0ttrA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BPrcr%2BfpvgZtLqPnGf9Nyvdk_TykaQOQ0y-xbxP2PuxCzY3MQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...