Re: [MW:34318] FILLER WIRE & ELECTRODE USE FOR A 333 Gr6 To A333 Gr6 , A 333 Gr6 To A106 Gr.B

Dear , 

from my understanding..  you mentioned consumable too can use , its all based on base metal tensile strength requirement regarding ..

Thanks & Regards 


Dinesh Baskaran 

Mail-Dinesh09nov@gmail.com

Mob- +91 9566261634 



On Tue, Jun 13, 2023 at 4:59 PM Ritesh Kumar Singh <riteshsiwan770@gmail.com> wrote:
Dear all 
Why we can't use Er70S2(spl) & E7018-1 ?

On Tue, 13 Jun 2023, 4:49 PM Mubashir khan <mubashirkhan9642@gmail.com> wrote:
Yes in our project we are using  ER80S-Ni1 & E7018-1 in Aramco project

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAALx7_K4Vukz0w17m0hYZy3jFedhXaDNZRVBD%2B-g1_krHhs9UQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-iLdiqP2GzS1_gq0ZhraftTLx%2BV7aEzVbksbLOhQ_us7w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMAJDVoqxUo2Q2G-jNCnHfBorjXDUcJCGWz%3D6RhUbYVgggsxWQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...