Re: [MW:34313] FILLER WIRE & ELECTRODE USE FOR A 333 Gr6 To A333 Gr6 , A 333 Gr6 To A106 Gr.B

You can use ER80S-Ni1  & E7018-1

Vào Th 3, 13 thg 6, 2023 vào lúc 06:11 PRABHUDAYAL MAHTO <massadmnistration@gmail.com> đã viết:
Dear all,

what is filler wire & Electrode use for  

Pipe material  - A 333 Gr6 To A333 Gr6  and    A 333 Gr6 To A106 Gr.B 


Thanks,

PRABHU  DAYAL 

+919566721541


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFbohSc1MwP0gq%2B%2BZt79JQgmmvv_XCXzNM0EyG0UjxvPzHvf2w%40mail.gmail.com.


--
Best & Regard
Pham Thanh Tinh
QC Manager
China National Chemical Engineering Third Co.LTD
South Ghawar Gas Separation Plant & Associated Facilities Project
Mobile phone +966. 556802308 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEVAJwY%3D6Zdk2BsLXd4RTLdB2A4jxWJP6rB2LjMJR98BzTiXEg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...