Monday, June 12, 2023

Re: [MW:34307] filler wire for Inconel 600

API RP 582.

On Mon, 12 Jun 2023 at 14:31, Hemant CPECC <hemant.cpecc@gmail.com> wrote:
Dear Pham,

Attached table from which Code have taken?

Thanks,

On Mon, Jun 12, 2023 at 3:12 PM Pham Thanh Tinh <tinhamem@gmail.com> wrote:
For your refence 



Vào Th 2, 12 thg 6, 2023 vào lúc 13:19 sujit kumar <sujitkumar19942@gmail.com> đã viết:
Dear all,

What filler wire we have to use to weld 
 INCONEL 600 TO INCONEL 600




Best Regards
sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMr0ieF94PAOgGi0VKuZybuoNmbto1gAXD6M6WspJ2G-g%40mail.gmail.com.


--
Best & Regard
Pham Thanh Tinh
QC Manager
China National Chemical Engineering Third Co.LTD
South Ghawar Gas Separation Plant & Associated Facilities Project
Mobile phone +966. 556802308 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEVAJwbVUAkz8Q4jhLuo65LmEnm5XYDJPnWbeYYncy4s%3Dukjdg%40mail.gmail.com.


--

Regards

Hemant Raychandel

QA/QC Engineer

CPECC

CHINA PETROLEUM ENGG. & CONSTRUCTION CORP. (M.E)

7th Floor, Onyx 2 Office Tower, Greens, Sheikh Zayed  Road, Dubai, U.A.E.

Tel: 04-3837942  |  Direct: 04-3837942  |  Mobile: +971 503316288

Email: hemant.cpecc@gmail.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMVKa9xeGnOz12yE8xDuB%3DmG31N8JHuo2rKBa6fC%2BwcJNBy7gQ%40mail.gmail.com.

The information in this email and any associated files is confidential to Veolia Water Technologies (SASU) and/or any affiliate thereof and may be legally privileged. For the herein purposes, "affiliate" means any legal entity, partnership, joint venture, equity, company, including in particular any and all subsidiary which, directly or indirectly, controls Veolia Water Technologies (SASU) and/or is under the control thereof and/or is under the control of the ultimate parent company thereof, and "control" means the ability to directly or indirectly, direct the affairs of a third party by means of ownership, contract or otherwise. It may also contain information that is subject to copyright or constitutes a trade secret. It is intended solely for the named recipient. Access to this email by anyone else is unauthorized.

If you are not the intended recipient, please note that any use, disclosure, copying, distribution of this email or any action taken or omitted to be taken in reliance on its prohibited.

Warning: Although this email and any attachment thereto are believed to be free from viruses, it is the responsibility of the recipient to ensure that they are virus free. No responsibility whatsoever is accepted by Veolia for any loss or damage arising from their receipt or opening.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPus-A4-U53iendba7vmvLbbegBwEMa%3DahNw5k2XHvevVsuLhw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...