Re: [MW:34296] Weld rejection rate for welders

Sir.

Targeted performance criteria on Weld Rejection Rate (WRR) for Welder and Welding Operator is 0.2% on linear method and 5% on weld joint method, with linear method being the over-riding factor. From the performance data the welders shall be categorized based on the linear Weld Repair Rate (WRR) as detailed in Appendix I. 

Vào Th 2, 12 thg 6, 2023 vào lúc 06:07 Ganesh R nair <ganeshrnair9@gmail.com> đã viết:
Dears,

As per SAEP - 324, linear weld rejection rate for welder is 0.2% max. But as per SAES W-10, maximum weld repair rate for welder is 2%. Which is correct. I am attaching screen shot of SAEP-324 and SAES W-10. Please advice.

Thanks & Regards,
Ganesh R

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ_8oJVEM1gb7b6ahL6ma0%3DndfA247w5OwNyOVKE73aidhdz3A%40mail.gmail.com.


--
Best & Regard
Pham Thanh Tinh
QC Manager
China National Chemical Engineering Third Co.LTD
South Ghawar Gas Separation Plant & Associated Facilities Project
Mobile phone +966. 556802308 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEVAJwb85Le8NjDc2jTT_%3Dusvjdch%2BW_TY1BNXCRkf59std3oQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...