YES it is for the Applicable positions Qualified.

Fillet welds shall be Qualified Separately. If your question is whether CJP groove weld qualifies Fillet weld then is is NO.

Fillet test shall be qualified as below.

Inline image


Inline image


Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Saturday, 10 June, 2023 at 05:38:01 pm IST, mithlesh kumar <mithleshmech47@gmail.com> wrote:


Dear James,

Attached table is for position qualification , Only in case of T,Y & K Type joint fillet can performed. Please correct me if I am wrong.


Thanks
Mithlesh

On Thursday, June 8, 2023 at 5:35:11 PM UTC+5:30 james gerald wrote:
Details like plate,  position etc.. required. Decode from the below snapshot of AWS D1.1

Inline image
Inline image



Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Thursday, 8 June, 2023 at 12:13:04 pm IST, Parminder Singh <parms...@gmail.com> wrote:


WPS qualified in CJP as per AWS D1.1 Ed 2020 

On Thu, Jun 8, 2023 at 11:57 AM Baqer Shabbeer <engb...@gmail.com> wrote:
Please share here qualification's and design code

On Wed, 7 Jun 2023 at 1:58 PM, Parminder Singh <parms...@gmail.com> wrote:
Dear Experts, 

Will CJP WPS qualify for Fillet Welds ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8bee16cf-540c-431a-a8b2-b5409547abd1n%40googlegroups.com.
--
Regards,
Baqer Shabbeer

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJBr9BGRACOA%2BKgyT7v9xDveXiOT9UOqJPgEamV0B91Doso78Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/bd5eed17-01c5-4f91-9a2c-d6fae0d74d9fn%40googlegroups.com
.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...