Saturday, June 10, 2023

Re: [MW:34285] Impact test requirement for Unlisted material (ASTM A707 L5 CL3)

For water service, Impact test not required.

On Sat, Jun 10, 2023 at 4:07 PM aravind roche <aravindroche@gmail.com> wrote:
Experts,

please advise below,  I believe because of our service temperature the impact test is not required, please guide me. 

PQR material - A707 L5 CL3 to API 5L Gr X65
Thickness coupon: 25.4 mm
WPS qualified range is : 5 to 50.8 mm
Design code : B31.3
Qualification Standard : ASME Sec IX
Our Project MDT : 0° to 90°C
Service : Water
PWHT : Yes
Pre heat : Yes

Aravind.A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ec3be245-165e-41a9-a0a2-40f333501774n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE%2B-gCb2WKtLXC6avG9fYAgjH7OdFbi2ManCX6V%2BwVtYzjOstw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...