what type of Joint is it.

1. Pressure vessel circum seam. seems unlikely due to huge thickness variation
2. Any Internal(like Ring) welding to the Clad.
3. Any External attachment to vessel.

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 19 January, 2023 at 02:08:51 pm GMT+3, Manikandan J <mechmani22@gmail.com> wrote:


Dear Experts,

We have a Vessel with the following MOC.(API RP 934 C)

Material 1 : SA 387 GR.11 CL.2 + SA 240 GR.347 (3.2 mm Cladded) -80 MM

Material 2 : SA 387 GR.11 CL.2 - 25 mm

Requesting your Technical inputs for PQR establishment.

Regards,
Manikandan
KSA

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmOB%3D_dMi2%3DyZhMJt1Bry7-ZgqbhZbcADcid8rGUrqvZJg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...