Re: [MW:33942] SA387 GR.11 CL.2 Vessel

It seems to be a plate material and do you have access to both sides of the joint. If so strip back 5 - 10 mm of clad inner side and weld the LAS using LAS WPS/PQR and do clad restoration using weld overlay PQR. 


On Thu, 19 Jan 2023 at 14:08, Manikandan J
<mechmani22@gmail.com> wrote:
Dear Experts,

We have a Vessel with the following MOC.(API RP 934 C)

Material 1 : SA 387 GR.11 CL.2 + SA 240 GR.347 (3.2 mm Cladded) -80 MM

Material 2 : SA 387 GR.11 CL.2 - 25 mm

Requesting your Technical inputs for PQR establishment.

Regards,
Manikandan
KSA

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmOB%3D_dMi2%3DyZhMJt1Bry7-ZgqbhZbcADcid8rGUrqvZJg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1102278266.1985987.1674133786641%40mail.yahoo.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...