Monday, January 16, 2023

Re: [MW:33926] Impact test requirements for PQR

Depends on Design code and applicable impact test requirements else you can use X46 to X46 pqr



On Mon, 16 Jan 2023 at 8:56, Karunakaran Karan
<karunaqc@gmail.com> wrote:
Hi experts,
   for perform PQR  on material API 5L X46 and X70 need separate PQR, X46-P1GR1  and X70 -P1 GR-3
                
   Thanks and regards,

     S.KARUNAKARAN,
      karunaqc@gmail.com
      91-6382279754
      91-7826930029(Whats app).







On Mon, Jan 16, 2023 at 11:09 AM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Some snapshot from sec ViiiDiv.I for reference.

Inline image

Inline image

Thanks & Regards

J.Gerald Jayakumar




On Sunday, 15 January, 2023 at 03:38:36 pm GMT+3, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Just to add. Charpy Impact test at MDMT (Minimum design Metal temperature) but if you perform at -48degC it can be used in the future.

API 5L X60 if ordered with special impact test requirement at -48degC then it will meet the requirement.

See below snap shot below.

Inline image


Thanks & Regards

J.Gerald Jayakumar




On Sunday, 15 January, 2023 at 03:32:24 pm GMT+3, Ritesh Kumar Singh <riteshsiwan770@gmail.com> wrote:


 thanks for replying
As per MTC of pipe, it's showing impact test at 0 degree C. Attached image for reference 

On Sun, 15 Jan 2023, 5:48 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Impact test shall be performed at -48degC

and pls ensure whether API 5L X60 is suitable for this temperature from the MTC

Thanks & Regards

J.Gerald Jayakumar




On Sunday, 15 January, 2023 at 02:36:04 pm GMT+3, Ritesh Kumar Singh <riteshsiwan770@gmail.com> wrote:


Dear expert's.

We are going to perform PQR  on material API 5L X60 (P1 G2 to P1 G2) 6" pipe.
Thk-21.95mm as per ASME sec 9.
Welding process-(GTAW Er70s-2(spl) + SMAW(E7018-1))


Client requirement are PWHT with impact test with other test as per code .
Kindly guide me for impact test temperature requirements.

We are qualifying this PQR  to weld rolled fittings of A537 CL1. thk 30 mm.
Design code ASME SEC 8 DIV1.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-hPkO6LTuoUw2%2BdBnYR1P8ex-Ti9FMwk_OWUr6V681zpA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/26135762.456028.1673784800697%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-j2b6NWVtzQ_XHrSQ6kzGi1QyMKM4D-iOXHse7EsgtveA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/624121096.911123.1673786247136%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/670180816.905141.1673787990390%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw9NbBOb4ueDJrrZkSb3JTSuh%2Bmq60UVxiDoC7zS4n%3Dsow%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1958138645.1041658.1673849418202%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...