Yes, PWPS means Pre-WPS. Based on that document PQR conducted, that needs mechanical test, root, face bend test and Tensile test. If test results are in acceptance limit than finally PWPS becomes WPS or final document ready for production welding.

On Tue, 10 Jan 2023, 07:59 Zacharias Rohith Joseph, <rohithjoseph18@gmail.com> wrote:
While using pre-qualified WPSs is it mandatory to do mechanical tests ? 

If yes , why are they called pre - qualified WPSs then ? 

Thanks 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bdd9b865-c130-4fb6-a025-01f5ec32f26fn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE%2B-gCaW8rSd3Ghu7io%3DHwek8wX4gJEN9BVSa0ybA%3DB26YNCLw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...