Re: [MW:33899] Set On Nozzle - Governing thickness for WPS

Set in, Set on , the governing thickness is nozzle^s thickness, if it is set through ,then it is Header thickness

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Jan 6, 2023 at 8:55 AM Jenish Mistry <jenishmistry1992@gmail.com> wrote:
Governing Thickness : 14 mm.

On Thu, Jan 5, 2023 at 2:23 PM Chintan Raval <chintan51@gmail.com> wrote:
Dear Expert,

Kindly advice,

For Pressure Vessel as per ASME Sec 8 Div 1,

Nozzle to Shell full penetration weld of Set on type nozzle, which is the governing thickness for wps selection i.e. thickness of nozzle or thickness of shell or both.

In a typical case,

Nozzle thickness 14 mm, needs to be welded on another nozzle of thickness 250 mm.

WPs available is with 5 mm to 200 mm range.

Is this wps can be used for set on type nozzle as it cover range of nozzle thickness

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdsS43ZLNQgO-s0Am8pQw5bJHg2X8SZBSTaZJXTy0zytLymFA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXbd_ex63w__LWo-%2BBxx-4fV0QSK52Pm%2BkCj0ZV%2BrQft4t6-w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM3xufBJouDO%2Bp09ggBW4y3J2oKKtFrqZa3rp%2BqO1wyjA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...