Re: [MW:33888] ASTM a36 and s275 jr

S275JR is an EN code material and considered as Unlisted Material. According to AWS D 1.1 it will not permit to weld ASTM A36 material.

But in AWS D1.1 Engineer (Client) has an Authority over AWS D1.1 code  and can permit to use this WPS.

Please take the issue with the Client.

Some Snap shots of code provided below.

Inline image

Inline image





Inline image

Thanks & Regards

J.Gerald Jayakumar



On Monday, 2 January, 2023 at 09:01:04 am IST, bavithran samuthralingam <bavithranviit@gmail.com> wrote:


Hi all 
i have a wps for the material S275 JR in aws d1.1 (ITS AN UNASSINED MATERIAL IN AWS D1.1)                 Can i use this wps for welding ASTM A36  ANY WELDING ENGINEER IN THIS GROUPS PLEASE GIVE ME AN IDEA

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0e8e5cc5-74e1-4c1c-9dd0-fd1bc79bed65n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...